DAK Americas Array™ 9921M PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer DAK Americas
Trade Name Array™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DAK Americas Array™ 9921M PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Array™ 9921M is unique copolymer particularly suited for use in the pharmaceutical and medical applications where clarity and gloss is desired. It is a medium intrinsic viscosity (IV) product that gives the end user superior processing and consistency.Typical Properties: Array™ 9921M offers excellent clarity and color, while maintaining good reheat characteristics for stretch blow molding. In addition it offers significantly reduced crystallization rates and a wide processing window. Array™ 9921M enables molding of thick walled parts while still retaining excellent clarity. It is capable of retaining properties under multiple sterilization processing techniques.Certification: Array™ 9921M is ideally suited for pharmaceutical and medical applications and is considered in compliance with the Food and Drug Administration (FDA) Food Contact Notification (FCN) 000635, USP Class VI and ISO 10993 Biocompatibility, US Pharmacopoeia and European Pharmacopoeia 3.1.15 and is supported via a Letter of Authorization for the FDA Drug Master File.Information provided by DAK Americas
Physical Properties Metric English Comments
Bulk Density 0.849 g/cc
0.0307 lb/in³
DAK-QAR-SOP-0018
Particle Size 3270 µm
3270 µm
Spherical Shape; DAK-QAR-SOP-0017
Particle Mesh Size 24 Mesh
24 Mesh
Fines: <0.05%, as packaged; DAK-QAR-SOP-0014
Viscosity Measurement 0.78 - 0.82
0.78 - 0.82
[dL/g], Intrinsic; DAK-QAR-SOP-0012
Crystallinity >= 35 %
>= 35 %
DAK-QAR-SOP-0016
Thermal Properties Metric English Comments
Melting Point 238 °C
460 °F
nominal; DAK-QAR-SOP-0016
Processing Properties Metric English Comments
Moisture Content <= 0.25 %
<= 0.25 %
DAK-QAR-SOP-0013; as packaged
Descriptive Properties Value Comments
Chip Size 53-73 chips/g
nominal, DAK-QAR-SOP-0015
Color >77.5 CIE
L*, BD-66060
-1.2 - 1.8 CIE
b*, BD-66060
Compounds <3 ppm
Acetaldehyde, DAK-QAR-SOP-0010