Cytec Thornel® P-650/42 Carbon Fiber/Epoxy Advanced Composite System

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite , Filled/Reinforced Thermoset
Manufacturer Cytec
Trade Name Thornel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec Thornel® P-650/42 Carbon Fiber/Epoxy Advanced Composite System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco and are now owned by Cytec.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2100 MPa
305000 psi
Tensile Modulus 170 GPa
24700 ksi
Compressive Yield Strength 1720 MPa
249000 psi
Shear Strength 120 MPa
17400 psi
Thermal Properties Metric English Comments
Thermal Conductivity 9.00 W/m-K
62.5 BTU-in/hr-ft²-°F