Material Notes:
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many specific potting and encapsulating applications such as modules, strain-sensitive components, transformers, and coils. All 2500 series systems exhibit excellent performance when exposed to adverse environments and temperature ranges between -55°C and +130°C.Cytec (Conap) EN-2521 Potting and Encapsulation AdhesiveU.L. recognized potting compounds. These systems are excellent choices where a device must eventually obtain U.L. approval. These systems have a U.L. Electrical Temperature Index Rating of 120°C. Refer to U.L. Index No. E69804.Passes Thermal Shock Test (10 Cycles, -65°C to 130°C)Non-Nutrient Fungus Resistance (MIL-STD-810B)Mix Ratio: 20/100 (by Weight)
Physical Properties Metric English Comments
Density 1.53 g/cc
0.0553 lb/in³
Cured
Water Absorption 0.19 %
0.19 %
24 hours
Water Absorption at Saturation 0.0055 %
0.0055 %
30 Days
Viscosity 4000 cP

@Temperature 25.0 °C
4000 cP

@Temperature 77.0 °F
Linear Mold Shrinkage 0.0071 cm/cm
0.0071 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 65 - 72
65 - 72
Tensile Strength, Ultimate 11.0 MPa
1600 psi
Elongation at Break 40 %
40 %
Thermal Properties Metric English Comments
CTE, linear 160 µm/m-°C

@Temperature 20.0 °C
88.9 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.272 W/m-K
1.88 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 1.20e+14 ohm-cm
<= 1.20e+14 ohm-cm
Surface Resistance 4.60e+13 ohm
4.60e+13 ohm
Dielectric Constant 4.3

@Frequency 1000 Hz
4.3

@Frequency 1000 Hz
Dielectric Strength 25.6 kV/mm

@Thickness 1.59 mm
650 kV/in

@Thickness 0.0625 in
Dissipation Factor 0.045

@Frequency 1000 Hz
0.045

@Frequency 1000 Hz
Arc Resistance >= 120 sec
>= 120 sec
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 100 °C
4.00 hour

@Temperature 212 °F
360 min

@Temperature 60.0 °C
6.00 hour

@Temperature 140 °F
10080 min

@Temperature 25.0 °C
168.0 hour

@Temperature 77.0 °F
Pot Life 60.0 - 80.0 min

@Temperature 25.0 °C
60.0 - 80.0 min

@Temperature 77.0 °F
1 lbm
Descriptive Properties Value Comments
Color Tan or Black