Custom Resins Vexel™ E20GF30 , 30% Glass Reinforced PET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Vexel™ E20GF30 , 30% Glass Reinforced PET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vexel™ E20GF30 is a 30% glass fiber reinforced, general purpose PET. Information provided by Custom Resins.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 145 MPa
21000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
ASTM D648