Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Custom Resins Norpex® GF3 PPE (Polyphenylene Ether), 30% Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 30% Glass Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Norpex® GF3 PPE (Polyphenylene Ether), 30% Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties for dry as molded samples.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Flexural Yield Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 6.90 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ASTM D648