Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Custom Resins Duratel™ MF13 Acetal Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Duratel™ MF13 Acetal Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Duratel™ MF13 is a 13 melt flow, general purpose acetal copolymer. Information provided by Custom Resins.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Linear Mold Shrinkage 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
Melt Flow 13 g/10 min
13 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 11 %
11 %
ASTM D638
Flexural Modulus 2.499 GPa
362.5 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
330 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ASTM D648