Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel , Tool Steel , Hot Work Steel
Manufacturer Crucible Steel
Trade Name Nu-Die®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and temper resistance, along with moderate wear resistance. It is air hardenable and is used in most applications in the heat treated condition at HRC 44-52. The normal tempering temperatures for Nu-Die V are quite high (>1000°F, 540°C), allowing it to retain its heat treated hardness and strength while in service at elevated temperatures. Nu-Die V may be used for tool temperatures up to about 1000°F (540°C) with brief exposures up to 1100°F (595°C), making it ideal for forging dies, hot extrusion tooling, and die casting dies. Crucible offers two premium versions, Nu-Die XL and Nu-Die ESR, for applications requiring critical polishability, improved heat check resistance and better transverse toughness.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 192 - 235
192 - 235
Annealed
Hardness, Rockwell C 40 - 42
40 - 42
Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C
51 - 53
51 - 53
Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C
Modulus of Elasticity 207 GPa
30000 ksi
Charpy Impact 14.0 J
10.3 ft-lb
Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 540°C
24.0 J
17.7 ft-lb
Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 20.0 - 95.0 °C
6.11 µin/in-°F

@Temperature 68.0 - 203 °F
11.5 µm/m-°C

@Temperature 20.0 - 205 °C
6.39 µin/in-°F

@Temperature 68.0 - 401 °F
12.6 µm/m-°C

@Temperature 20.0 - 540 °C
7.00 µin/in-°F

@Temperature 68.0 - 1000 °F
Thermal Conductivity 26.0 W/m-K

@Temperature 95.0 °C
180 BTU-in/hr-ft²-°F

@Temperature 203 °F
27.7 W/m-K

@Temperature 315 °C
192 BTU-in/hr-ft²-°F

@Temperature 599 °F
Shrinkage -0.0600 %

@Treatment Temp. 540 - 620 °C
-0.0600 %

@Treatment Temp. 1000 - 1150 °F
Tempered 540-620°C
Component Elements Properties Metric English Comments
Carbon, C 0.40 %
0.40 %
Chromium, Cr 5.2 %
5.2 %
Iron, Fe 91.15 %
91.15 %
As Remainder
Molybdenum, Mo 1.3 %
1.3 %
Silicon, Si 1.0 %
1.0 %
Vanadium, V 0.95 %
0.95 %
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved