Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Crucible Steel MAXEL® 3-1/2 (Brake Die) Free-Machining Alloy Steel, AISI 4150 S

Category Metal , Ferrous Metal , Alloy Steel , AISI 4000 Series Steel
Manufacturer Crucible Steel
Trade Name Maxel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel MAXEL® 3-1/2 (Brake Die) Free-Machining Alloy Steel, AISI 4150 S.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MAXEL 3-1/2 free-machining alloy steel provides a good combination of heat treated properties and machinability. This alloy steel is manufactured under close quality control to an ASTM grain size of 5 to 8. It is suitable for service applications where strength, toughness, and hardness are required.MAXEL 3-1/2 can be supplied in the heat treated and stress relieved condition to a hardness of BHN 269/321. This results in not only an economic advantage, but also minimizes distortion normally encountered in heat treating finished parts.Information provided by Crucible Industries
Physical Properties Metric English Comments
Density 7.81 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 170 - 212
170 - 212
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 11.7 µm/m-°C

@Temperature 21.1 - 93.3 °C
6.50 µin/in-°F

@Temperature 70.0 - 200 °F
12.6 µm/m-°C

@Temperature 21.1 - 204 °C
7.00 µin/in-°F

@Temperature 70.0 - 400 °F
Component Elements Properties Metric English Comments
Carbon, C 0.50 %
0.50 %
Chromium, Cr 0.65 %
0.65 %
Iron, Fe 97 %
97 %
as balance
Manganese, Mn 1.25 %
1.25 %
Molybdenum, Mo 0.15 %
0.15 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S 0.080 %
0.080 %
Chemical Properties Metric English Comments
Critical Temperature 738 °C
1360 °F