Material Notes:
CSM 420 XL is the workhorse premium quality stainless mold steel designed for applications requiring a combination of corrosion resistance and wear resistance. It is double melted for the microstructural uniformity and microcleanliness levels that are required for critical applications and highly polished finishes. Molds made from CSM 420XL are resistant to the rust and pitting from water cooling or condensation, and can go in and out of extended storage with little maintenance. At HRC 48-52, CSM 420XL also has the highest hardness of the stainless mold steels, and it offers the greatest compressive strength and the best wear resistance.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.64 g/cc
0.276 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 51.3
51.3
Hardening Temperature- 1010°C; Tempering Temperature- 454°C
52.5
52.5
Hardening Temperature- 1030°C; Tempering Temperature- 454°C
53.2
53.2
Hardening Temperature- 1050°C; Tempering Temperature- 454°C
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 10.3 µm/m-°C

@Temperature 0.000 - 100 °C
5.72 µin/in-°F

@Temperature 32.0 - 212 °F
10.8 µm/m-°C

@Temperature 0.000 - 320 °C
6.00 µin/in-°F

@Temperature 32.0 - 608 °F
Thermal Conductivity 24.9 W/m-K

@Temperature 93.0 °C
173 BTU-in/hr-ft²-°F

@Temperature 199 °F
Shrinkage -0.0400 %
-0.0400 %
Component Elements Properties Metric English Comments
Carbon, C 0.38 %
0.38 %
Chromium, Cr 13.6 %
13.6 %
Iron, Fe 84.47 %
84.47 %
As Remainder
Manganese, Mn 0.50 %
0.50 %
Silicon, Si 0.75 %
0.75 %
Vanadium, V 0.30 %
0.30 %