Category Metal , Ferrous Metal , Tool Steel
Manufacturer Crucible Steel
Trade Name CPM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel CPM® Nu-Die® EZ Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CRUCIBLE CPM Nu-Die EZ is a new, patented die and mold steel designed for service as die casting dies and plastic injection molds. It is supplied in the prehardened condition, and is easily machined using conventional chip-making methods.This unique die and mold steel provides:Freedom from Distortion in Heat TreatmentFreedom from Worry over Heat Treatment QualityFreedom from EDM DamageCPM Nu-Die EZ is based upon the chemical composition of AISI H13 hot work steel to which sulfur has been added to provide machinability in the prehardened condition. It is manufactured by the Crucible Particle Metallurgy (CPM) Process which permits the addition of sulfur without detrimental effects on tool performance. Unlike the sulfides which form in conventionally-produced, resulfurized H13, the sulfides in this steel are small and uniformly distributed.Information provided by Crucible Industries
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 45
45
Modulus of Elasticity 207 GPa
30000 ksi
Charpy Impact 12.2 J
9.00 ft-lb
V-notch
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C

@Temperature 21.1 - 93.3 °C
6.10 µin/in-°F

@Temperature 70.0 - 200 °F
11.5 µm/m-°C

@Temperature 21.1 - 204 °C
6.40 µin/in-°F

@Temperature 70.0 - 400 °F
12.2 µm/m-°C

@Temperature 21.1 - 427 °C
6.80 µin/in-°F

@Temperature 70.0 - 800 °F
12.6 µm/m-°C

@Temperature 21.1 - 538 °C
7.00 µin/in-°F

@Temperature 70.0 - 1000 °F
13.1 µm/m-°C

@Temperature 21.1 - 649 °C
7.30 µin/in-°F

@Temperature 70.0 - 1200 °F
Thermal Conductivity 2.16 W/m-K

@Temperature 93.3 °C
15.0 BTU-in/hr-ft²-°F

@Temperature 200 °F
2.31 W/m-K

@Temperature 316 °C
16.0 BTU-in/hr-ft²-°F

@Temperature 600 °F
Component Elements Properties Metric English Comments
Carbon, C 0.36 %
0.36 %
Chromium, Cr 5.5 %
5.5 %
Iron, Fe 90.2 %
90.2 %
as balance
Manganese, Mn 0.35 %
0.35 %
Molybdenum, Mo 1.6 %
1.6 %
Silicon, Si 1.0 %
1.0 %
Sulfur, S 0.17 %
0.17 %
Vanadium, V 0.85 %
0.85 %