Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Crucible Compaction Metals P/M N690 Corrosion Resistant Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Crucible Compaction Metals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Compaction Metals P/M N690 Corrosion Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
P/M N690 (chemically, UNS N06690) is produced by the state-of-the-art Crucible P/M process: inert gas atomization, coupled with consolidation by hot isostatic pressing and/or extrusion. The advanced Crucible powder consolidation operation guarantees a fully dense, fine grained product. Crucible custom crafted parts can be machined in less time and with less tool wear than those produced from conventional 690 material.P/M N690 gives engineers and designers great flexibility in design. It is available in standard mill forms and as billet, bar and tubing, near net shapes and clad components and hollows. The use of near net shapes can decrease the amount of material used and reduces the costs of fabricating a finished part.Advantages:Excellent corrosion resistance High strength Weldability Machinability Chemical homogeneity Near net shape Thermal stabilityInformation provided by Crucible Compaction Metals.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 862 MPa

@Temperature 23.0 °C
125000 psi

@Temperature 73.4 °F
Tensile Strength, Yield 469 MPa

@Strain 0.200 %
68000 psi

@Strain 0.200 %
As-Consolidated; At Room Temperature
Elongation at Break 39 %

@Temperature 23.0 °C
39 %

@Temperature 73.4 °F
Reduction of Area 60 %

@Temperature 23.0 °C
60 %

@Temperature 73.4 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.040 %
<= 0.040 %
Chromium, Cr 28 - 31 %
28 - 31 %
Copper, Cu <= 0.50 %
<= 0.50 %
Iron, Fe 7.0 - 11 %
7.0 - 11 %
Manganese, Mn <= 0.50 %
<= 0.50 %
Nickel, Ni 56.445 - 63.445 %
56.445 - 63.445 %
as balance
Silicon, Si <= 0.50 %
<= 0.50 %
Sulfur, S <= 0.015 %
<= 0.015 %
Copyright © lookpolymers.com All Rights Reserved