Material Notes:
Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °C
154 °F
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
Vicat Softening Point 140 °C
284 °F
50°C/h 50N
Glass Transition Temp, Tg 0.000 °C
32.0 °F
10°C/min
Processing Properties Metric English Comments
Melt Temperature 230 °C
446 °F
Injection Molding
Mold Temperature 35.0 °C
95.0 °F
Injection Molding
Injection Pressure 45.0 MPa
6530 psi