Material Notes:
Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.00 MPa

@Strain 50.0 %
1160 psi

@Strain 50.0 %
Elongation at Break >= 50 %
>= 50 %
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 224 µm/m-°C

@Temperature 20.0 °C
124 µin/in-°F

@Temperature 68.0 °F
Vicat Softening Point 128 °C
262 °F
50°C/h 50N
Glass Transition Temp, Tg -27.0 °C
-16.6 °F
10°C/min
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+10 ohm-cm
5.00e+10 ohm-cm
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Dielectric Constant 5.1

@Frequency 1e+6 Hz
5.1

@Frequency 1e+6 Hz
6.6

@Frequency 100 Hz
6.6

@Frequency 100 Hz
Dielectric Strength 14.8 kV/mm
376 kV/in
Dissipation Factor 0.025

@Frequency 100 Hz
0.025

@Frequency 100 Hz
0.075

@Frequency 1e+6 Hz
0.075

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Melt Temperature 205 °C
401 °F
Injection Molding
Mold Temperature 30.0 °C
86.0 °F
Injection Molding
Injection Pressure 45.0 MPa
6530 psi