Covestro Texin® 285 Urethane Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Covestro
Trade Name Texin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Texin® 285 Urethane Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.00 MPa

@Strain 50.0 %
725 psi

@Strain 50.0 %
Elongation at Break >= 50 %
>= 50 %
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 150 µm/m-°C

@Temperature 20.0 °C
83.3 µin/in-°F

@Temperature 68.0 °F
Vicat Softening Point 91.0 °C
196 °F
50°C/h 50N
Glass Transition Temp, Tg -42.0 °C
-43.6 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL Recognized
V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
UL Recognized
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+9 ohm-cm
8.00e+9 ohm-cm
Surface Resistance 5.00e+11 ohm
5.00e+11 ohm
Dielectric Constant 5.6

@Frequency 1e+6 Hz
5.6

@Frequency 1e+6 Hz
6.5

@Frequency 100 Hz
6.5

@Frequency 100 Hz
Dielectric Strength 17.5 kV/mm
445 kV/in
Dissipation Factor 0.025

@Frequency 100 Hz
0.025

@Frequency 100 Hz
0.060

@Frequency 1e+6 Hz
0.060

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Melt Temperature 200 °C
392 °F
Injection Molding
Mold Temperature 30.0 °C
86.0 °F
Injection Molding
Injection Pressure 45.0 MPa
6530 psi