Covestro Petlon® 8535 Semi-Crystalline PET, 35% Mineral/Glass Fiber  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Petlon® 8535 Semi-Crystalline PET, 35% Mineral/Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Impact Modified: Excellent Electrical Properties, High Heat ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperature: 495-530°F, Mold Temperature: 195-250°F)Petlon® is manufactured by Albis Plastics Corporation and is a registered trademark of Bayer Corporation.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Water Absorption 0.040 %
0.040 %
(24 hr); ASTM D570
Moisture Absorption at Equilibrium 0.24 %
0.24 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 112.4 MPa
16300 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 166.2 MPa
24110 psi
ASTM D790
Flexural Modulus 9.17 GPa
1330 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 18.5 µm/m-°C

@Temperature 20.0 °C
10.3 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 212 °C
414 °F
ASTM D648
Vicat Softening Point >= 225 °C
>= 437 °F
ASTM D1525
Flammability, UL94 HB
HB
0.125 in; Albis Internal Test
Electrical Properties Metric English Comments
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Processing Properties Metric English Comments
Melt Temperature 257 - 277 °C
495 - 531 °F
Injection
Mold Temperature 91.0 - 121 °C
196 - 250 °F