Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Makrolon® DP 1-1413 Polycarbonate, Gamma Radiation Stabilized

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Gamma Radiation Resistant
Manufacturer Covestro
Trade Name Makrolon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Makrolon® DP 1-1413 Polycarbonate, Gamma Radiation Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium viscosity grade suitable for sterilization with hot-air and gamma radiation, specially suitable for medical equipment (dialyser housings).Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Water Absorption 0.35 %
0.35 %
Saturation in water
Moisture Absorption at Equilibrium 0.15 %
0.15 %
Equilibrium at 50% RH
Water Absorption at Saturation 0.35 %
0.35 %
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 6.0 %
6.0 %
Tensile Modulus 2.40 GPa
348 ksi
Charpy Impact Unnotched NB
NB
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
Vicat Softening Point 145 °C
293 °F
Users viewing this material also viewed the following: