Covestro Makrofol® ID 4-4 white Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Covestro
Trade Name Makrofol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Makrofol® ID 4-4 white Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Makrofol ID 4-4 white is available in four different color grades and is the top choice inlay-material in cards. Surface: Fine matte/Fine matte Available in various standard thicknesses between 105 and 300µm, other thicknesses on request. Available as Roll and sheetsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Descriptive Properties Value Comments
Availability Europe
Near East/Africa
North America
South and Central America