Covestro Makrofol® BL 6-2 820803 Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Covestro
Trade Name Makrofol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Makrofol® BL 6-2 820803 Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Makrofol BL 6-2 820803 is a dazzle-free, scratch resistant extruded light diffusion film based on the Bayer MaterialScience High Tech Polycarbonate Makrolon. The color is black translucent, the surface texture is one side fine velvet, one side very fine matte. It is available in a standard thickness of 400 micron, other thicknesses on request. UL94 VTM-2, FMVSS 302As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Descriptive Properties Value Comments
Availability Europe
Near East/Africa
North America
South and Central America