Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Makroblend® DP 7665 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Covestro
Trade Name Makroblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Makroblend® DP 7665 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Modulus 4.20 GPa
609 ksi
ISO 527-1/-2
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
234 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 260 - 280 °C
500 - 536 °F
270 °C
518 °F
Injection Molding; ISO 294
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
70.0 °C
158 °F
Injection Molding; ISO 10724
Injection Velocity 200 mm/sec
7.87 in/sec
ISO 294
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Near East/Africa
North America
South and Central America
Feature Release agent
Form Pellets
Process Injection Molding