Covestro Desmopan® W DP89043D Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® W DP89043D Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
3s; ISO 868
Hardness, Shore D 43
43
15s; ISO 868
Tensile Strength at Break 39.0 MPa
5660 psi
ISO 527-1/-2
Tensile Strength, Yield 39.0 MPa
5660 psi
parallel; ISO 527-3
12.0 MPa

@Strain 100 %
1740 psi

@Strain 100 %
ISO 527-1/-2
18.0 MPa

@Strain 300 %
2610 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 11
11
mm³; ISO 4649
Compression Set 41 %

@Temperature 70.0 °C
41 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
India
North America