Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Desmopan® DP 8795A S043 Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 8795A S043 Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
3s; ISO 868
Hardness, Shore D 41
41
15s; ISO 868
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-1/-2
Tensile Strength, Yield 50.0 MPa
7250 psi
parallel; ISO 527-3
10.0 MPa

@Strain 100 %
1450 psi

@Strain 100 %
ISO 527-1/-2
24.0 MPa

@Strain 300 %
3480 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 17
17
mm³; ISO 4649
Compression Set 21 %

@Temperature 23.0 °C
21 %

@Temperature 73.4 °F
ISO 815
45 %

@Temperature 70.0 °C
45 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
India
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved