Material Notes:
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
3s; ISO 868
Hardness, Shore D 65
65
15s; ISO 868
Tensile Strength at Break 64.0 MPa
9280 psi
ISO 527-1/-2
Tensile Strength, Yield 64.0 MPa
9280 psi
parallel; ISO 527-3
29.0 MPa

@Strain 100 %
4210 psi

@Strain 100 %
ISO 527-1/-2
45.0 MPa

@Strain 300 %
6530 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 30
30
mm³; ISO 4649
Descriptive Properties Value Comments
Availability Asia Pacific
India
Feature Release agent
Form Pellets
Process Injection Molding