Material Notes:
Coating gradedoes not contain any anti-hydrolysis agentfood contact applications are possiblecontact our HSEQ departmentApplicationTextile coatingPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Melt
1.21 g/cc
0.0437 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
3s; ISO 868
Hardness, Shore D 50
50
15s; ISO 868
Abrasion 70
70
mm³; ISO 4649
Compression Set 26 %

@Temperature 23.0 °C
26 %

@Temperature 73.4 °F
ISO 815
69 %

@Temperature 70.0 °C
69 %

@Temperature 158 °F
ISO 815
Thermal Properties Metric English Comments
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Thermal Conductivity 0.139 W/m-K
0.965 BTU-in/hr-ft²-°F
Melt
Processing Properties Metric English Comments
Melt Temperature 190 - 220 °C
374 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Ejection Temperature 50.0 °C
122 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America
Eff. thermal diffusivity (m²/s) 7.98E-08