Material Notes:
Extrusion- and injection molding gradesuitable for extrusion blow moldinghigh melt stabilityvery large processing windowApplicationBellowsInjection molded engineering partsO-stringsHosesnon-reinforcedAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
3s; ISO 868
Hardness, Shore D 40
40
15s; ISO 868
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-1/-2
Tensile Strength, Yield 50.0 MPa
7250 psi
parallel; ISO 527-3
8.50 MPa

@Strain 100 %
1230 psi

@Strain 100 %
ISO 527-1/-2
18.0 MPa

@Strain 300 %
2610 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 35
35
mm³; ISO 4649
Compression Set 24 %

@Temperature 23.0 °C
24 %

@Temperature 73.4 °F
ISO 815
47 %

@Temperature 70.0 °C
47 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America