Material Notes:
Desmopan 150 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
DIN 53505
Hardness, Shore D 50
50
DIN 53505
Elongation at Break >= 50 %
>= 50 %
Nominal
Compression Set 25 %
25 %
70 hr; 22°C
55 %

@Temperature 70.0 °C
55 %

@Temperature 158 °F
24 hr
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 210 µm/m-°C

@Temperature 20.0 °C
117 µin/in-°F

@Temperature 68.0 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Surface Resistance 2.00e+12 ohm
2.00e+12 ohm
Dielectric Constant 4.6

@Frequency 1e+6 Hz
4.6

@Frequency 1e+6 Hz
6.0

@Frequency 100 Hz
6.0

@Frequency 100 Hz
Dielectric Strength 14.1 kV/mm
358 kV/in
Dissipation Factor 0.029

@Frequency 100 Hz
0.029

@Frequency 100 Hz
0.066

@Frequency 1e+6 Hz
0.066

@Frequency 1e+6 Hz