Material Notes:
Uses: Suitable for the production of parts: for example: insulators, bushing insulators, components of switchgear cabinets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Water Absorption 0.050 %
0.050 %
Saturation in water
Water Absorption at Saturation 0.050 %
0.050 %
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 88.0 MPa
12800 psi
Elongation at Break 1.3 %
1.3 %
Tensile Modulus 9.10 GPa
1320 ksi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.0 µm/m-°C

@Temperature 20.0 °C
18.9 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 34.0 µm/m-°C

@Temperature 20.0 °C
18.9 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg 140 °C
284 °F
Oxygen Index 35 %
35 %
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Dielectric Constant 4.3

@Frequency 1e+6 Hz
4.3

@Frequency 1e+6 Hz
4.5

@Frequency 100 Hz
4.5

@Frequency 100 Hz
Dielectric Strength 32.0 kV/mm
813 kV/in
Dissipation Factor 0.013

@Frequency 100 Hz
0.013

@Frequency 100 Hz
0.015

@Frequency 1e+6 Hz
0.015

@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
600 V