Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Bayflex® 110-50 Polyurethane Elastomeric RIM, 15% Milled Glass Reinforced, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Glass Filled , Rubber or Thermoset Elastomer (TSE)
Manufacturer Covestro
Trade Name Bayflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayflex® 110-50 Polyurethane Elastomeric RIM, 15% Milled Glass Reinforced, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption at Saturation 2.6 %
2.6 %
240 hours; Bayer Test
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
Bayer Test
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Ultimate 19.0 MPa
2760 psi
ASTM D638/D412
Elongation at Break 200 %
200 %
ASTM D638/D412
Flexural Modulus 0.690 GPa
100 ksi
ASTM D790
Izod Impact, Notched 4.30 J/cm
8.06 ft-lb/in
ASTM D256
Tear Strength 110 kN/m
628 pli
Die C; ASTM D624
Thermal Properties Metric English Comments
CTE, linear 79.2 µm/m-°C

@Temperature 20.0 °C
44.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696