Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Glass Filled
Manufacturer Covestro
Trade Name Baydur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Baydur® STR/C-405 IMR Polyurethane Composite SRIM Foam, 45% Glass Filled, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Contains continuous strand fiberglass mat.0.118 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
Bayer Test
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 103 MPa
14900 psi
ASTM D638/D412
Flexural Yield Strength 178 MPa
25800 psi
ASTM D790
Flexural Modulus 8.30 GPa
1200 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 26.0 µm/m-°C

@Temperature 20.0 °C
14.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 212 °C
414 °F
ASTM D648