Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Baydur® 60 Polyurethane

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer Covestro
Trade Name Baydur®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Baydur® 60 Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Rigid integral skin polyurethane foam for engineering components. The integral distribution of density gives a higher flexural modulus. If required, the property level can be improved by increasing the density.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 0.600 g/cc
0.0217 lb/in³
Water Absorption 0.30 %
0.30 %
Saturation in water
Water Absorption at Saturation 0.30 %
0.30 %
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.0 MPa
3050 psi
Elongation at Break 7.0 %
7.0 %
Tensile Modulus 0.800 GPa
116 ksi
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.0 µm/m-°C

@Temperature 20.0 °C
40.6 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 73.0 µm/m-°C

@Temperature 20.0 °C
40.6 µin/in-°F

@Temperature 68.0 °F
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 7.00e+14 ohm-cm
7.00e+14 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 10.0 kV/mm
254 kV/in
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: