Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Bayblend® T85 Polycarbonate + ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Covestro
Trade Name Bayblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayblend® T85 Polycarbonate + ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose injection molding gradeVicat/B 120 temperature = 131°Chigh impact and notched impact strengthPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
0.980 g/cc

@Temperature 260 °C
0.0354 lb/in³

@Temperature 500 °F
Melt
Water Absorption 0.70 %
0.70 %
Similar to ISO 62
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Similar to ISO 62
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 260 °C
12 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-1/-2
Elongation at Yield 4.7 %
4.7 %
ISO 527-1/-2
Tensile Modulus 2.30 GPa
334 ksi
ISO 527-1/-2
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
41.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Specific Heat Capacity 1.73 J/g-°C
0.413 BTU/lb-°F
Melt
Thermal Conductivity 0.154 W/m-K
1.07 BTU-in/hr-ft²-°F
Melt
Deflection Temperature at 0.46 MPa (66 psi) 127 °C
261 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 109 °C
228 °F
ISO 75-1/-2
Vicat Softening Point 129 °C
264 °F
50°C/h 50N; ISO 306
Flammability, UL94 HB

@Thickness 0.900 mm
HB

@Thickness 0.0354 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
IEC 60250
3.1

@Frequency 100 Hz
3.1

@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
889 kV/in
IEC 60243-1
Dissipation Factor 0.0020

@Frequency 100 Hz
0.0020

@Frequency 100 Hz
IEC 60250
0.0085

@Frequency 1.00e+6 Hz
0.0085

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 225 V
225 V
IEC 60112
Processing Properties Metric English Comments
Melt Temperature 240 - 280 °C
464 - 536 °F
260 °C
500 °F
Injection Molding; ISO 294
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
80.0 °C
176 °F
Injection Molding; ISO 10724
Ejection Temperature 130 °C
266 °F
Injection Velocity 240 mm/sec
9.45 in/sec
ISO 294
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
North America
South and Central America
Eff. thermal diffusivity (m²/s) 9.08E-08
Feature Heat stabilised or stable to heat
Release agent
Form Pellets
Process Injection Molding
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved