Covestro Bayblend® R-T 60 Polycarbonate/ABS Blend

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Covestro
Trade Name Bayblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayblend® R-T 60 Polycarbonate/ABS Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Recycled grade in which carefully reclaimed old parts and production rejects and/or scrap from all processes of manufacturing or processing undergo material recycling. Slightly decreased impact strength compared to BAYBLEND T 64/T 65/T 65MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Water Absorption 0.70 %
0.70 %
Saturation in water
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Equilibrium at 50% RH
Water Absorption at Saturation 0.70 %
0.70 %
Melt Flow 19 g/10 min

@Load 5.00 kg,
Temperature 260 °C
19 g/10 min

@Load 11.0 lb,
Temperature 500 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 4.0 %
4.0 %
Tensile Modulus 2.00 GPa
290 ksi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 85.0 µm/m-°C

@Temperature 20.0 °C
47.2 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
Vicat Softening Point 118 °C
244 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Oxygen Index 23 %
23 %
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Constant 2.0

@Frequency 100 Hz
2.0

@Frequency 100 Hz
2.9

@Frequency 1e+6 Hz
2.9

@Frequency 1e+6 Hz
Dielectric Strength 24.0 kV/mm
610 kV/in
Dissipation Factor 0.0040

@Frequency 100 Hz
0.0040

@Frequency 100 Hz
0.0070

@Frequency 1e+6 Hz
0.0070

@Frequency 1e+6 Hz
Comparative Tracking Index 300 V
300 V