Mechanical Properties Metric English Comments
Flexural Strength 20.7 MPa
3000 psi
Compressive Strength 34.5 MPa
5000 psi
Thermal Properties Metric English Comments
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 °C
4.00 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 2.02 W/m-K
14.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1090 °C
2000 °F