Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cotronics Duralco™ 128 500°F (260°C) Ceramic Filled Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Cotronics
Trade Name Duralco™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Duralco™ 128 500°F (260°C) Ceramic Filled Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ceramic filled, electrically resistant adhesive and potting compound. The ceramic fillers provide both high thermal conductivity and high dielectric strength. Cures at room temperature. Curing can be accelerated with mild heat.
Physical Properties Metric English Comments
Viscosity 15000 cP
15000 cP
Thermal Properties Metric English Comments
Thermal Conductivity 4.32 W/m-K
30.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Processing Properties Metric English Comments
Cure Time 960 - 1440 min

@Temperature 93.3 °C
16.0 - 24.0 hour

@Temperature 200 °F
Users viewing this material also viewed the following: