Cotronics Duralco™ 127 400°F (200°C) Graphite Filled Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Cotronics
Trade Name Duralco™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Duralco™ 127 400°F (200°C) Graphite Filled Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One component, graphite filled epoxy for low cost production applications. Can be used with automatic dispensing equipment.
Physical Properties Metric English Comments
Viscosity 50000 cP
50000 cP
Thermal Properties Metric English Comments
Thermal Conductivity 3.60 W/m-K
25.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
400 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.020 ohm-cm
0.020 ohm-cm
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 162 °C
0.167 hour

@Temperature 324 °F
Users viewing this material also viewed the following: