Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cossa Polimeri ESTAPROP KUR 1010 TG05 Polypropylene, 5% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Mineral Reinforced
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTAPROP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cossa Polimeri ESTAPROP KUR 1010 TG05 Polypropylene, 5% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP copolymer 5% mineral fillerElastomer modified, very high impact strength at low temperatureInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.012 - 0.015 cm/cm
0.012 - 0.015 in/in
ASTM D 955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D 638
Elongation at Break >= 200 %
>= 200 %
ASTM D 638
Tensile Modulus 1.00 GPa
145 ksi
ASTM D 638
Flexural Modulus >= 0.800 GPa
>= 116 ksi
ASTM D 790
Izod Impact, Notched 10.0 J/cm

@Temperature -20.0 °C
18.7 ft-lb/in

@Temperature -4.00 °F
ASTM D 638
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point >= 50.0 °C

@Load 5.00 kg
>= 122 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in