Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cossa Polimeri ESTAPROP 1540 GFC V0 H Flame Retardant Polypropylene, 20% Glass Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler , Polypropylene, Flame Retardant
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTAPROP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cossa Polimeri ESTAPROP 1540 GFC V0 H Flame Retardant Polypropylene, 20% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP with 20% glass fiber reinforcedFlame retardant class UL V0 and class M2 according to NL P92-507Information provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D 792
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
ASTM D 638
Elongation at Break 3.0 %
3.0 %
ASTM D 638
Flexural Modulus 5.00 GPa
725 ksi
ASTM D 790
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point 120 °C

@Load 5.10 kg
248 °F

@Load 11.2 lb
50°C/hr; ASTM D 1525
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
I.E.C. 695-2-1