Cossa Polimeri ESTABLEND 7500 V0 HF Flame Retardant PC - ABS

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTABLEND
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cossa Polimeri ESTABLEND 7500 V0 HF Flame Retardant PC - ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D 955
Melt Flow 25 g/10 min

@Load 5.00 kg,
Temperature 240 °C
25 g/10 min

@Load 11.0 lb,
Temperature 464 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 54.0 MPa
7830 psi
ASTM D 638
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D 638
Elongation at Break 40 %
40 %
ASTM D 638
Flexural Modulus 2.50 GPa
363 ksi
ASTM D 790
Izod Impact, Notched 5.50 J/cm

@Temperature 0.000 °C
10.3 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
6.00 J/cm

@Temperature 23.0 °C
11.2 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Hot Ball Pressure Test 105 °C
221 °F
I.E.C. 335-1
Vicat Softening Point 110 °C

@Load 5.00 kg
230 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
116 °C

@Load 0.999 kg
241 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Glow Wire Test 960 °C
1760 °F
I.E.C. 695-2-1