Material Notes:
Biodegradable plastic for the extrusion of disposablesCertified for food contactInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D 792
Melt Flow <= 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
<= 3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Elongation at Break >= 30 %
>= 30 %
ASTM D 638
Flexural Modulus 2.80 GPa
406 ksi
ASTM D 790
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
120°C/hr; ASTM D 648
Processing Properties Metric English Comments
Dry Time 3.00 hour

@Temperature 50.0 °C
3.00 hour

@Temperature 122 °F