CoorsTek StatSafe™ ZDC-W Static Dissipative Zirconia

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer CoorsTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek StatSafe™ ZDC-W Static Dissipative Zirconia.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specialized StatSafe™ ESD-safe zirconia combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffness, wear and corrosion resistance, low thermal expansion, and dimensional stability. Typical applications include: end effectors, ESD sensitive component handling, data storage drive components, and data storage drive manufacturing tools.
Physical Properties Metric English Comments
Density 5.91 g/cc
0.214 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 200 GPa
29000 ksi
Flexural Strength 650 MPa
94300 psi
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C
5.56 µin/in-°F
Thermal Conductivity 3.50 W/m-K
24.3 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 - 1.00e+7 ohm-cm
1.00e+6 - 1.00e+7 ohm-cm
Descriptive Properties Value Comments
Color White