Material Notes:
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.Data Provided by the manufacturer, CoorsTek, Inc.
Physical Properties Metric English Comments
Density 3.18 g/cc
0.115 lb/in³
ASTM C20
Water Absorption 0.00 %
0.00 %
ASTM 373
Particle Size 8.0 µm
8.0 µm
Thin Section Crystal Size
Mechanical Properties Metric English Comments
Knoop Microhardness 24
24
1000 g
Modulus of Elasticity 375 GPa
54400 ksi
ASTM C848
Flexural Strength 540 MPa
78300 psi
ASTM F417
Poissons Ratio 0.21
0.21
ASTM C848
Fracture Toughness 6.90 MPa-m½
6.28 ksi-in½
Notched Beam
Shear Modulus 155 GPa
22500 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 3.30 µm/m-°C

@Temperature 25.0 - 1000 °C
1.83 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
Specific Heat Capacity 0.800 J/g-°C
0.191 BTU/lb-°F
ASTM E1269
Thermal Conductivity 80.0 W/m-K
555 BTU-in/hr-ft²-°F
ASTM C408
Maximum Service Temperature, Air 1000 °C
1830 °F
No Load
Descriptive Properties Value Comments
Color Black