CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal

Category Polymer
Manufacturer CoorsTek
Trade Name PolyGlyde™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-running situations, leak-tight material, greater durability, less wear debris – runs cleaner, broader resistance to chemical attack, suitable for fluid and gas applications, lapping of seal face not necessary, and exceptionally stable.
Physical Properties Metric English Comments
Specific Gravity 2.01 g/cc
2.01 g/cc
ASTM-D792
Deformation 5.9 %

@Pressure 13.8 MPa,
Temperature 25.6 °C
5.9 %

@Pressure 2000 psi,
Temperature 78.0 °F
24 hrs.; ASTM-D621
9.9 %

@Pressure 4.14 MPa,
Temperature 260 °C
9.9 %

@Pressure 600 psi,
Temperature 500 °F
24 hrs.; ASTM-D621
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.4 MPa
1800 psi
ASTM-D1457
Elongation at Break 60 %
60 %
ASTM-D1457
Flexural Strength 17.2 MPa
2500 psi
ASTM-F417
Flexural Modulus 0.0117 GPa
1.70 ksi
ASTM-D790
Compressive Strength 48.3 MPa
7000 psi
ASTM-C773
Thermal Properties Metric English Comments
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
ASTM-D696
Thermal Conductivity 0.807 W/m-K
5.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Descriptive Properties Value Comments
Color Black