Material Notes:
Oxygen ionic conductor for extreme-stress and extreme-thermal-shock environments
Physical Properties Metric English Comments
Density 4.90 g/cc
0.177 lb/in³
ASTM-C 20
Water Absorption 0.00 %
0.00 %
ASTM-373
Mechanical Properties Metric English Comments
Hardness, Rockwell 45 N 85
85
Flexural Strength 350 MPa
50800 psi
MOR; ASTM-F417
Fracture Toughness 3.50 MPa-m½
3.19 ksi-in½
Notched Beam
Thermal Properties Metric English Comments
CTE, linear 8.30 µm/m-°C

@Temperature 25.0 - 1000 °C
4.61 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM-C372
Thermal Conductivity 23.0 W/m-K
160 BTU-in/hr-ft²-°F
ASTM-C408
Maximum Service Temperature, Air 1500 °C
2730 °F
NO-LOAD COND.
Descriptive Properties Value Comments
Color White
Permeability Gas tight
Thermal Shock Resistance (°C) 500
ΔTc