ConocoPhillips Hydroclear Diamond Class® 32/46 Rotary Compressor Fluid

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear Diamond Class®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear Diamond Class® 32/46 Rotary Compressor Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear Diamond Class Rotary Compressor Fluids are designed to lubricate rotary screw compressors operating in air compression service. These semisynthetic products combine high-stability, highly processed base oils with the protection provided by a custom additive package. This blend of components results in products that combine exceptional air compressor performance and a moderate price.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.853 g/cc
0.0308 lb/in³
Viscosity Measurement 108
108
Viscosity Index
Saybolt Viscosity at 100°F 187 SUS
187 SUS
Saybolt Viscosity at 210°F 47.5 SUS
47.5 SUS
Kinematic Viscosity at 40°C (104°F) 40 cSt
40 cSt
Kinematic Viscosity at 100°C (212°F) 6.5 cSt
6.5 cSt
Thermal Properties Metric English Comments
Pour Point <= -37.2 °C
<= -35.0 °F
Flash Point 232 °C
450 °F
Chemical Properties Metric English Comments
Total Acid Number 0.010
0.010