Material Notes:
Description: Conoco Brick Grease is a hard, amber-colored, smooth-textured, lithium-based grease made in block or brick form. Brick Grease provides a high melting point block grease with good heat resistance. It is designed for the lubrication of open heavy-duty bearings equipped with open well top feed grease collars, such as: Kiln, trunnion and support wall bearings; Ball, tube, rod and comped mill bearings; Paper machine dryer section; Cement mills, jack shaft bearings, crushers, rolling mills, rubber compounding mills, etc.; Kiln dryers; DehydratorsInformation provided by ConocoPhillips.
Physical Properties Metric English Comments
Viscosity Measurement 81
81
Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 450 - 550 SUS
450 - 550 SUS
Base Oil Property
Saybolt Viscosity at 210°F 55 - 65 SUS
55 - 65 SUS
Base Oil Property
Kinematic Viscosity at 40°C (104°F) 105 cSt
105 cSt
Base Oil
Kinematic Viscosity at 100°C (212°F) 10.5 cSt
10.5 cSt
Base Oil
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 45 - 65
45 - 65
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 129 °C
265 °F
Minimum Service Temperature, Air -12.2 °C
10.0 °F
Dropping Point 196 °C
385 °F
Descriptive Properties Value Comments
Color Medium Amber
Soap Type (Thickener) Lithium