Compuestos Dominicanos SA manufactures polycom VN product series for the extrusion of printable sheets and banners providing excellent stability, ease of processing and excellent printable characteristics of finished products.Applications : Sheets and banners Appearance: Natural pelletsInformation provided by Compuestos Dominicanos
Physical Properties Metric English Comments
Specific Gravity 1.36 - 1.40 g/cc
1.36 - 1.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92

@Time 15.0 sec
88 - 92

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D412
Elongation at Break 596 %
596 %
ASTM D412