Material Notes:
Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resistance and low temperature applications. Products in different colors, hardness, and finish are available for any specific need. Compuestos Dominicanos SA also manufactures specialty compounds that offer high resistance to abrasion for shoe soles.Oil resistance/abrasion resistance shoe sole Appearance: Black PelletsInformation provided by Compuestos Dominicanos
Physical Properties Metric English Comments
Specific Gravity 1.15 - 1.19 g/cc
1.15 - 1.19 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 54

@Time 15.0 sec
50 - 54

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 10.0 MPa
1450 psi
ASTM D412
Elongation at Break 420 %
420 %
ASTM D412