Clariant Renol PPSSP0001 Polyphenylene Sulfide, Glass Fiber and Bead Filled

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PPSSP0001 Polyphenylene Sulfide, Glass Fiber and Bead Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Processing Properties Metric English Comments
Melt Temperature 299 - 321 °C
570 - 610 °F
Mold Temperature 51.7 - 79.4 °C
125 - 175 °F
Dry Time 2 - 4 hour
2 - 4 hour
to ensure moisture level is less than 0.05%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.000 - 0.345 MPa
0.000 - 50.0 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 50 rpm
20 - 50 rpm