Clariant Renol BR7039G30 Nylon 6, 30% Glass Fiber, bondable to TPU

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol BR7039G30 Nylon 6, 30% Glass Fiber, bondable to TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Filler Content 30 %
30 %
ASTM D2584
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 105.0 MPa
15230 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 180 MPa
26100 psi
ASTM D790
Flexural Modulus 0.724 GPa
105 ksi
ASTM D790
Processing Properties Metric English Comments
Melt Temperature 238 - 260 °C
460 - 500 °F
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 0.827 MPa
50.0 - 120 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm