Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.003924 GPa

@Temperature 110 °C,
Time 86400 sec
0.5691 ksi

@Temperature 230 °F,
Time 24.0 hour
0.00981 GPa

@Temperature 1500 °C,
Time 10800 sec
1.42 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
24.5 MPa

@Temperature 1500 °C,
Time 10800 sec
3560 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Shrinkage 0.00 %

@Temperature 110 °C,
Time 86400 sec
0.00 %

@Temperature 230 °F,
Time 24.0 hour
0.10 %

@Temperature 1500 °C,
Time 10800 sec
0.10 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 75 %
75 %
SiO2 20 %
20 %
Descriptive Properties Value Comments
Installation Method Troweling
Main Applications Tundish Repair
Material Required for Estimating (kg/?) 2,500
Water Required for Casting(%) 11