Chosun Refractories SR Blast Furnace Runner Refractory

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SR Blast Furnace Runner Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.66 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.0961 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
2.68 g/cc

@Temperature 110 °C,
Time 86400 sec
0.0968 lb/in³

@Temperature 230 °F,
Time 24.0 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0047088 GPa

@Temperature 110 °C,
Time 86400 sec
0.68296 ksi

@Temperature 230 °F,
Time 24.0 hour
0.01393 GPa

@Temperature 1500 °C,
Time 10800 sec
2.020 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 0.1268 MPa

@Temperature 1500 °C,
Time 10800 sec
18.39 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
36.2 MPa

@Temperature 110 °C,
Time 86400 sec
5250 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 67 %
67 %
Descriptive Properties Value Comments
Chemical Analysis(%),SiC+C 17
Installation Method Casing Vibration
Main Applications Slag Iron runner
Material Required for Estimating (kg/?) 2,850
Water Required for Casting(%) 6.5